UnholyWardenG t1_ivm51w0 wrote

Yes, but it takes ages, and could potentially alter the structural integrity of the pot, depending on how bad the pitting is.

I wet sand the area with varying grits to level the surface , then polish. Give it a good scub with hot water and soap and it's good to go. If it's deeply pitted, i.e. more that 1/8th the total thickness of the parent metal, then unfortunately it can't be polished out.

My 5qt Magnalite took me about 6-7 hours using a mix of hand sanding and a drill with sanding disks. Looks fantastic now. 👌